LSS D7 is a high-carbon, high-chromium, air-hardening stainless tool steel with great wear resistance. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information on wear resistance as well as heat treating and machining. Filing Code: TS-725. Producer or source: Latrobe Specialty Steel Company.