Abstract

Formadur 2311 is a plastic mold steel with good polishability. It is comparable to P-20. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on surface qualities as well as heat treating and joining. Filing Code: TS-700. Producer or source: Schmolz + Bickenbach USA Inc..