Abstract

Uddeholm Vancron 40 offers an excellent combination of galling resistance and adhesive wear resistance, which should be used in cold-work applications where the predominant failure mechanisms are adhesive wear or galling. Typical applications include blanking and forming, cold extrusion, deep drawing, and powder pressing. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating, machining, surface treatment, and powder metal forms. Filing Code: TS-687. Producer or source: Böhler-Uddeholm North America.