Abstract

Orvar 2M is a conventional tool steel of overall good ductility, toughness, weldability, and machinability. The alloy has the best overall product consistency for conventionally produced AISI H13 type tool steels. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-661. Producer or source: Böhler-Uddeholm North America.