Abstract

Whitebear is an 8% Cr, cold work tool steel with lower carbon than similar grades, which improves the impact toughness. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on wear resistance as well as heat treating and machining. Filing Code: TS-652. Producer or source: Timken Latrobe Steel.