Abstract

Thyrodur 2767/2767 Supra is a cold-work tool steel with high hardenability for punching tools. Thyrodur 2767 Supra is the electroslag remelted version. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating. Filing Code: TS-651. Producer or source: Schmolz + Bickenbach USA Inc.