Abstract

Finkl DC is a single-vacuum melted AISI H13 type material made by the vacuum arc degassing (VAD) process. The vanadium content of 1% in addition to a high chromium (Cr 5%) and molybdenum (Mo 1.4%) promotes hot strength and wear resistance. This datasheet provides information on composition. It also includes information on heat treating. Filing Code: TS-614. Producer or source: A. Finkl & Sons Company.