Abstract

CRU-WEAR is an air hardening tool steel with wear resistance greater than D2 and toughness approaching A2. Applications include blades, punches and dies. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating and joining. Filing Code: TS-592. Producer or source: Crucible.