Boehler W302 ISOBLOC is a premium grade H13 tool steel with a good combination of toughness, heat-checking resistance, temperature resistance, and high-temperature strength. This datasheet provides information on composition, physical properties, and hardness. It also includes information on high temperature performance as well as heat treating, machining, joining, and surface treatment. Filing Code: TS-579. Producer or source: Böhler.