Abstract

Boehler S7MQ is an improved version of an AISI S7 tool steel. Typical usage is for plastic molding and cold-work applications. This datasheet provides information on composition and hardness. It also includes information on heat treating and machining. Filing Code: TS-578. Producer or source: Böhler.