Abstract

Uddeholm HOLDER is a free-machining chromium-molybdenum alloyed tool steel supplied in the prehardened condition. Applications include parts and molds for plastic and rubber. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on heat treating, machining, and joining. Filing Code: TS-575. Producer or source: Uddeholm Corporation.