Abstract

Vanadis 23 is a Cr-Mo-W-Va alloyed high-speed steel made by powder metallurgy. The tool steel offers an excellent combination of wear resistance and toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on heat treating, machining, and surface treatment. Filing Code: TS-561. Producer or source: Uddeholm Corporation. See also Alloy Digest TS-552, March 1997.