Abstract

THYROTHERM 2713 is a tough hot work die steel with retention to tempering. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating, machining, joining, and surface treatment. Filing Code: TS-516. Producer or source: Thyssen Specialty Steels Inc.