Abstract

RED CUT SUPERIOR J is a tungsten-type of hot-work tool and die steel; in fact, it is the 18 tungsten-4 chromium-1 vanadium high-speed composition with carbon lowered to provide more toughness. It is characterized by high red hardness and good resistance to abrasion. It is recommended for applichations in which hardness must be maintained at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-410. Producer or source: Teledyne Vasco.