MOSIL is intended for applications requiring high toughness and resistance to shock loading. It is recommended for severe and repeated impacts in service. It has an excellent combination of hardness and toughness to withstand the high stresses in service and to resist abrasion and wear. Normally, it is hardened by austenitizing and quenching in oil. Among the many uses of Mosil are hand chisels, hammers, rivet sets, concrete breakers and heavy-duty punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, joining, and surface treatment. Filing Code: TS-400. Producer or source: Teledyne Vasco.