Abstract

CARPENTER No. 882 is a 5% chromium hot-work tool steel designed particularly for applications requiring extreme toughness combined with good red hardness. It also has found cold-work applications. It can be used at strength levels in excess of 260,000 psi (18,300 kg/cm2). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-339. Producer or source: Carpenter.