FAGERSTA M-2 is a widely used molybdenum-base high-speed steel. It is suitable for all general-purpose cutting-tool applications and it has an excellent combination of toughness and wear resistance. Its many applications include boring tools, chisels, lathe tools and shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and surface treatment. Filing Code: TS-337. Producer or source: Fagersta Steels Inc..