Abstract
SUPER MOTUNG 33 is one of the heavy-duty high-speed steels. It is recommended for machining materials of high hardness. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-322. Producer or source: Cyclops Corporation.