Carpenter No. 484FM is an air-hardening steel capable of hardening throughout in heavy sections. It is recommended for heavy duty tool and die service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-160. Producer or source: Carpenter.