VASCO-MC is a medium carbon, chromium, molybdenum mold and cavity steel recommended for molds where good machinability and high surface finishes are desired. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-143. Producer or source: Vanadium Alloys Steel Corporation.