Abstract

Latrobe BR-3 is a very high-carbon, chromium, vanadium, molybdenum die steel for cold working applications. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-133. Producer or source: Latrobe Steel Company.