Abstract

HYCC is a high-carbon high-chromium tool steel having high wear and abrasion resistance combined with non-deforming characteristics. It is particularly adaptable for blanking dies and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-132. Producer or source: Crucible Steel Company of America.