Abstract

TRI-TUNG is a high-carbon, high-chromium tool steel recommended for tools requiring high hardness and exceptional resistance to abrasive wear. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-125. Producer or source: Uddeholm Company of America Inc..