Abstract

LEHIGH-S is the oil-hardening type of high-carbon high-chromium tool and die steel, having high abrasion resistance and very little change in size and shape during heat treatment. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-119. Producer or source: Bethlehem Steel Corporation.