Abstract

Hotform V is a medium-carbon, 5% chromium hot work tool and die steel having improved wear resistance and hot hardness at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-113. Producer or source: Vanadium Alloys Steel Company.