Abstract

BETHLEHEM Cr-Mo-W is a general purpose hot work tool and die steel having excellent resistance to wear, shock, and drastic changes in temperature. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-57. Producer or source: Bethlehem Steel Corporation.