OTTAWA-60 is a high-carbon high-vanadium alloy steel which has been specifically designed to deep draw and form stainless steel without pickup or galling and to give the ultimate in wear resistance for this application. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-34. Producer or source: Allegheny Ludlum Corporation.