Abstract

CHAMPALOY is a tough, oil-hardening, electric furnace alloy steel suitable for general purpose applications. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-21. Producer or source: Crucible Steel Company of America. Originally published June 1954, revised January 1965.