Abstract

Ulbrich Titanium Grade 1 (UNS R50250) is an unalloyed commercially pure titanium. It is one of the softest and the most ductile of the commercially pure grades, and exhibits excellent formability. It has excellent corrosion resistance and is mainly used in marine and chemical industries where the parts are exposed to very harsh environments. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming. Filing Code: Ti-165. Producer or source: Ulbrich Stainless Steels & Special Metals, Inc.

This content is only available as a PDF.
You do not currently have access to this content.