ATI 6-2-4-2 alloy is a near-alpha high strength titanium alloy. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ti-158. Producer or source: Allegheny Technologies Inc..