Abstract

Timetal Exhaust XT is a lean alloy, but exhibits good corrosion resistance and higher strength than needed for automotive exhaust. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming. Filing Code: Ti-156. Producer or source: Timet.