Abstract

Timetal Grade 12 is a lean alloy, but exhibits better corrosion resistance and higher strength than grade 2. This datasheet provides information on composition, physical properties, tensile properties. and bend strength. It also includes information on corrosion resistance as well as forming. Filing Code: Ti-153. Producer or source: Timet.