TIMETAL 65A is a general purpose grade of commercially pure titanium that has excellent corrosion resistance to highly oxidating to mildly reducing environments, including chlorides, and an excellent strength-to-weight ratio. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: TI-147. Producer or source: Timet.