Abstract

Timetal 54M has better machinability than TI-6Al-4V with comparable properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on forming, heat treating, and machining. Filing Code: TI-146. Producer or source: Timet.