Abstract

Titanium shows outstanding resistance to seawater and marine atmospheres. It is also resistant to attack by hot metallic chloride solutions, sodium and potassium hypochlorite, and chlorine dioxide. The metal is resistant to attack by hot nitric acid at concentrations up to 80% and is not attacked by sulfuric acid. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: TI-122. Producer or source: Timet.