Abstract

Allegheny Ludlum CP chemically pure titanium alloys feature low density and high strength-to-weight ratio. They are suitable for many corrosive chemical environments, including oxidizing chloride solutions, seawater, and chlorine-based bleaches. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming and joining. Filing Code: TI-115. Producer or source: Allegheny Ludlum Corporation. Originally published September 2000, corrected November 2000.