Abstract

Ti-45 Niobium offers resistance to oxidizing media, including reduced pyrophoric, and ignition characteristics. Applications include aqueous pressure oxidation of ores. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. Filing Code: TI-106. Producer or source: Teledyne Wah Chang Albany.