TIMETAL 1100, a near alpha alloy, was developed for elevated temperature use around 1100 F (600 C). The alloy is to be used in the beta processed condition. The alloy offers the highest combination of strength, creep resistance, fracture toughness, and stability of any commercially available titanium alloy. This datasheet provides information on composition, physical properties, and tensile properties as well as creep and fatigue. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: TI-104. Producer or source: Timet.