ALLVAC 8A1-1Mo-1V alloy is predominantly alpha in microstructure, aluminum being the alpha stabilizing component and giving the alloy the lowest density of all commercial titanium based materials. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-97. Producer or source: Teledyne Allvac.