RMI 25 is a grade of commercially pure titanium. It has a guaranteed minimum yield strength of 25,000 psi with good ductility and formability. Its yield strength is about the same as that of the annealed austenitic stainless steels of lowest yield strength. It has excellent resistance to corrosion by many chemicals, seawater and marine atmospheres. It is used for equipment in the chemical and marine industries. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-76. Producer or source: RMI Company.