Abstract

Ti-6A1-2Sn-4Zr-6Mo is a high-strength titanium-base alloy having excellent properites in the intermediate temperature range. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-64. Producer or source: Titanium Metals Corporation of America.