KENTANIUM K151A is a titanium carbide cermet having high heat and oxidation resistance along with very high wear and abrasion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on machining and joining. Filing Code: Ti-49. Producer or source: Kennametal Inc..