Abstract

Republic RS-110A is a titanium alloy containing manganese as its principle alloying element. The alloy is a medium strength, highly formable sheet alloy which has been used extensively as an aircraft structural material. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-35. Producer or source: Republic Steel Corporation, Titanium Division.