Abstract

KBI-6 is a tantalum-base alloy with added tungsten for strengthening. It is used in the chemical process industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ta-8. Producer or source: Cabot Corporation.