Abstract

UGI 4362 is an austenitic ferritic duplex stainless steel with good strength and corrosion resistance. It has superior yield strength, ultimate tensile strength, and corrosion resistance compared with 316L stainless. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: SS-1289. Producer or source: Schmolz + Bickenbach USA Inc..