Abstract

MTEK Super 20-32Nb is a solid solution Fe-Cr-Ni casting alloy with good high temperature strength. This datasheet provides information on composition, physical properties, microstructure, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting, heat treating, machining, and joining. Filing Code: SS-1252. Producer or source: MetalTek International.