Outokumpu 2507 is a super duplex stainless with molybdenum and high mechanical properties. It is designed for demanding applications for both corrosion resistance and strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1215. Producer or source: Outokumpu Stainless AB, Avesta Research Centre.