Abstract

UGI 209 is an austenitic stainless steel with high corrosion resistance and a low magnetic permeability. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-1192. Producer or source: Schmolz + Bickenbach USA Inc..