Abstract

Ugima 4571 is a general-purpose, corrosion-resistant austenitic stainless steel with added titanium for stabilization of the weld. The machining productivity increase is 15–30% compared with the regular grade 1.4571 stainless. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1183. Producer or source: Schmolz + Bickenbach USA Inc..