Abstract

Mecasteel 17-4 is a precipitation hardening grade with good toughness and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SS-1181. Producer or source: Industeel USA, LLC.